The difference in the basal spacing (8.79Å) and a higher mass loss (6.2%) in the temperature range of 200-750°C of naproxen-bentonite (N-bentonite) comparing to that of Unye bentonite (UB) signified the existence of thermally stable organic species in the interlamellar space of the bentonite clay. The asymmetric OCO- stretching band (1607cm-1) of N-bentonite became stronger in the temperature interval of 100-400°C as a result of binding via the CO group of the ligand to exchangeable cation and/or water molecule whereas the OH bending peak of water (1633cm-1) and the CC stretching vibration of aromatic ring (1531cm-1) became weaker on thermal treatment. The effect of ionic strength on the desorption of naproxen species and the related kinetic data revealed that the release mechanism at pH=7.4 is unrestricted diffusion controlled and governed by the repulsive interactions between the bentonite surface and the negatively charged species. The pore structure characteristics of the bentonite samples corresponding to the surface area, pore volume and pore size were determined by using the conventional analysis of the nitrogen adsorption-desorption isotherms. © 2011 Elsevier B.V.

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/ebyu/15732Resmi atıflarda kullanılan kalıcı adres
DOI
https://doi.org/10.1016/j.cej.2011.09.027Yayıncı resmi DOI adresi
Tam Kayıt
AlanDeğerDil
dc.contributor.authorTabak, A.
dc.contributor.authorYilmaz, N.
dc.contributor.authorEren, E.
dc.contributor.authorCaglar, B.
dc.contributor.authorAfsin, B.
dc.contributor.authorSarihan, A.
dc.date.accessioned2026-10-18T20:30:34.793584035Z
dc.date.available2026-10-18T20:30:34.793584035Z
dc.date.issued2011
dc.description.abstractThe difference in the basal spacing (8.79Å) and a higher mass loss (6.2%) in the temperature range of 200-750°C of naproxen-bentonite (N-bentonite) comparing to that of Unye bentonite (UB) signified the existence of thermally stable organic species in the interlamellar space of the bentonite clay. The asymmetric OCO- stretching band (1607cm-1) of N-bentonite became stronger in the temperature interval of 100-400°C as a result of binding via the CO group of the ligand to exchangeable cation and/or water molecule whereas the OH bending peak of water (1633cm-1) and the CC stretching vibration of aromatic ring (1531cm-1) became weaker on thermal treatment. The effect of ionic strength on the desorption of naproxen species and the related kinetic data revealed that the release mechanism at pH=7.4 is unrestricted diffusion controlled and governed by the repulsive interactions between the bentonite surface and the negatively charged species. The pore structure characteristics of the bentonite samples corresponding to the surface area, pore volume and pore size were determined by using the conventional analysis of the nitrogen adsorption-desorption isotherms. © 2011 Elsevier B.V.
dc.identifier.doi10.1016/j.cej.2011.09.027
dc.identifier.eissn1873-3212
dc.identifier.endpage288
dc.identifier.issn1385-8947
dc.identifier.issue1
dc.identifier.scopus2-s2.0-80053963988
dc.identifier.startpage281
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/ebyu/15732
dc.identifier.volume174
dc.identifier.wosWOS:000296950300036
dc.language.isoen
dc.publisherELSEVIER SCIENCE SA
dc.relation.ispartofChemical Engineering Journal
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectFTIR
dc.subjectNaproxen
dc.subjectSurface area
dc.subjectTG/DTA/DSC
dc.subjectUnye-bentonite
dc.subjectXRD
dc.subjectDesorption
dc.subjectDyes
dc.subjectGas adsorption
dc.subjectIonic strength
dc.subjectpH effects
dc.subjectStretching
dc.subjectStructural analysis
dc.subjectNaproxens
dc.subjectBentonite
dc.titleStructural analysis of naproxen-intercalated bentonite (Unye)
dc.typeArticle
dspace.entity.typePublication
rdl.citation.scopus78
rdl.citation.wos73
rdl.source.indexSCOPUS
rdl.source.indexWOS
rdl.wos.indexScience Citation Index Expanded (SCI-EXPANDED)