Investigation of temperature, catalyst thickness and substrate effects in In2O3 nanostructures

ArticleAçık Erişim

Özet

This study successfully synthesized In2O3 nanotowers (NTs), nanowires (NWs), nanochains (NChs) and nanocrystals (NCs) on n-type Si(100) and quartz substrates at temperature of 900–1000 °C by using Au catalysts via the Chemical Vapor Deposition (CVD) technique. The analyses of experimental results revealed that In2O3 nanostructures (NSs) grew in different morphologies due to variable parameters, such as temperature, thickness of catalyst and substrate type. This was because these In2O3 NSs were formed by both the Vapor-Liquid-Solid (VLS) and the Vapor-Solid (VS) growth mechanisms. For instance, In2O3 NTs and NChs were formed by the VLS growth mechanism; In2O3 NCs were formed by the VS growth mechanism and In2O3 NWs were formed by both the VLS and VS growth mechanisms. Morphology and crystal structures were identified through X-Ray Diffraction (XRD), High Resolution Transmission Electron Microscopy (HRTEM), Field Emission Scanning Electron Microscopy (FESEM) and Energy Dispersive X-Ray Spectroscopy (EDS). Moreover, photoluminescence (PL) peaks of In2O3 NSs were measured to be 367 nm, 470 nm, and 630 nm at room temperature (RT). These measurement results indicated that structural, morphological, compositional and optical properties of synthesized In2O3 NSs correlated with growth parameters. © 2017 Elsevier Ltd

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/ebyu/14096Resmi atıflarda kullanılan kalıcı adres
DOI
https://doi.org/10.1016/j.jpcs.2017.08.035Yayıncı resmi DOI adresi
Tam Kayıt
AlanDeğerDil
dc.contributor.authorTuzluca, Fatma Nur
dc.contributor.authorYesilbag, Yasar Ozkan
dc.contributor.authorErtugrul, Mehmet
dc.date.accessioned2026-10-18T20:28:52.519426108Z
dc.date.available2026-10-18T20:28:52.519426108Z
dc.date.issued2017
dc.description.abstractThis study successfully synthesized In2O3 nanotowers (NTs), nanowires (NWs), nanochains (NChs) and nanocrystals (NCs) on n-type Si(100) and quartz substrates at temperature of 900–1000 °C by using Au catalysts via the Chemical Vapor Deposition (CVD) technique. The analyses of experimental results revealed that In2O3 nanostructures (NSs) grew in different morphologies due to variable parameters, such as temperature, thickness of catalyst and substrate type. This was because these In2O3 NSs were formed by both the Vapor-Liquid-Solid (VLS) and the Vapor-Solid (VS) growth mechanisms. For instance, In2O3 NTs and NChs were formed by the VLS growth mechanism; In2O3 NCs were formed by the VS growth mechanism and In2O3 NWs were formed by both the VLS and VS growth mechanisms. Morphology and crystal structures were identified through X-Ray Diffraction (XRD), High Resolution Transmission Electron Microscopy (HRTEM), Field Emission Scanning Electron Microscopy (FESEM) and Energy Dispersive X-Ray Spectroscopy (EDS). Moreover, photoluminescence (PL) peaks of In2O3 NSs were measured to be 367 nm, 470 nm, and 630 nm at room temperature (RT). These measurement results indicated that structural, morphological, compositional and optical properties of synthesized In2O3 NSs correlated with growth parameters. © 2017 Elsevier Ltd
dc.description.sponsorshipThis study was supported by the Scientific Research Project Unit (Project Number: FBA-2016-370 ) of Basic Science Application and Research Center at Erzincan University. Authors thank Dr. Atilla AYDINLI (Uludag University), Murat GURE (Advanced Research Laboratory of Bilkent University) and Mustafa GULER (UNAM-National Nanotechnology Research Center) for their valuable contributions. Authors also acknowledge the contributions of the National Nanotechnology Research Center of Bilkent University Institute of Materials Science and Nanotechnology.
dc.identifier.doi10.1016/j.jpcs.2017.08.035
dc.identifier.eissn1879-2553
dc.identifier.endpage446
dc.identifier.issn0022-3697
dc.identifier.scopus2-s2.0-85028546408
dc.identifier.startpage439
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/ebyu/14096
dc.identifier.volume111
dc.identifier.wosWOS:000412609200057
dc.language.isoen
dc.publisherElsevier Ltd
dc.relation.ispartofJournal of Physics and Chemistry of Solids
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectFESEM
dc.subjectHRTEM
dc.subjectIndium oxide
dc.subjectNanostructures
dc.subjectPhotoluminescence
dc.subjectCatalysts
dc.subjectChemical vapor deposition
dc.subjectElectron microscopy
dc.subjectEnergy dispersive spectroscopy
dc.subjectField emission microscopes
dc.subjectOptical properties
dc.subjectScanning electron microscopy
dc.subjectSubstrates
dc.subjectX ray diffraction
dc.subjectX ray spectroscopy
dc.subjectChemical vapor depositions (CVD)
dc.subjectEnergy dispersive X ray spectroscopy
dc.subjectField emission scanning electron microscopy
dc.subjectMorphology and crystal structures
dc.subjectVLS growth mechanism
dc.subjectHigh resolution transmission electron microscopy
dc.titleInvestigation of temperature, catalyst thickness and substrate effects in In2O3 nanostructures
dc.typeArticle
dspace.entity.typePublication
rdl.citation.scopus3
rdl.citation.wos3
rdl.source.indexSCOPUS
rdl.source.indexWOS
rdl.wos.indexScience Citation Index Expanded (SCI-EXPANDED)