Effect of Expanded Perlite Aggregate Plaster on the Behavior of High-Temperature Reinforced Concrete Structures

ArticleAçık Erişim

Özet

Polyurethane-based materials, which are widely used in exterior cladding, pose a great risk for buildings because they can easily catch fire at temperatures as low as 50–65 °C. Thus, different materials are needed to ensure that structures exposed to high temperatures do not have any stability problems. In this study, expanded perlite aggregate plaster (EPAP) was produced to eliminate the negative effects that may occur in buildings exposed to high temperatures. High temperature tests were carried out on test plates of different thicknesses to determine the effect of plaster thickness under high temperatures. In order to compare the effects of high temperatures, a test sample of normal aggregate plaster (NAP), which is widely used in buildings, was prepared. In the high temperature test, the temperature values on the back surfaces of the EPAP (≈115 °C) test plates were approximately 3 times lower than the temperature values of the NAP (≈350 °C) test plate. It can be said that structural stability loss and durability problems may occur in structures covered with NAP in a high-temperature environment, and that no negative effect will occur in terms of structural stability and durability problems in structures covered with EPAP in high temperature environments. © 2023 by the authors.

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/ebyu/12491Resmi atıflarda kullanılan kalıcı adres
DOI
https://doi.org/10.3390/buildings13020384Yayıncı resmi DOI adresi
Tam Kayıt
AlanDeğerDil
dc.contributor.authorUlusu, İsmet
dc.contributor.authorKurnuç Seyhan, Aslıhan
dc.date.accessioned2026-10-18T20:27:23.272058713Z
dc.date.available2026-10-18T20:27:23.272058713Z
dc.date.issued2023
dc.description.abstractPolyurethane-based materials, which are widely used in exterior cladding, pose a great risk for buildings because they can easily catch fire at temperatures as low as 50–65 °C. Thus, different materials are needed to ensure that structures exposed to high temperatures do not have any stability problems. In this study, expanded perlite aggregate plaster (EPAP) was produced to eliminate the negative effects that may occur in buildings exposed to high temperatures. High temperature tests were carried out on test plates of different thicknesses to determine the effect of plaster thickness under high temperatures. In order to compare the effects of high temperatures, a test sample of normal aggregate plaster (NAP), which is widely used in buildings, was prepared. In the high temperature test, the temperature values on the back surfaces of the EPAP (≈115 °C) test plates were approximately 3 times lower than the temperature values of the NAP (≈350 °C) test plate. It can be said that structural stability loss and durability problems may occur in structures covered with NAP in a high-temperature environment, and that no negative effect will occur in terms of structural stability and durability problems in structures covered with EPAP in high temperature environments. © 2023 by the authors.
dc.identifier.doi10.3390/buildings13020384
dc.identifier.eissn2075-5309
dc.identifier.issn2075-5309
dc.identifier.issue2
dc.identifier.scopus2-s2.0-85149241945
dc.identifier.startpage384
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/ebyu/12491
dc.identifier.volume13
dc.identifier.wosWOS:000938472800001
dc.language.isoen
dc.publisherMDPI
dc.relation.ispartofBuildings
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectexpanded perlite
dc.subjecthigh temperature
dc.subjectplaster
dc.subjectstructure durability
dc.subjectstructure stability
dc.titleEffect of Expanded Perlite Aggregate Plaster on the Behavior of High-Temperature Reinforced Concrete Structures
dc.typeArticle
dspace.entity.typePublication
rdl.citation.scopus9
rdl.citation.wos7
rdl.oa.statusgold
rdl.source.indexSCOPUS
rdl.source.indexWOS
rdl.wos.indexScience Citation Index Expanded (SCI-EXPANDED)