Investigation of mechanical and wear properties of five (5) different CAD/CAM restorative materials; [Beş (5) farklı CAD / CAM restoratif malzemelerin mekanik ve aşınma özelliklerinin incelenmesi]

ArticleAçık Erişim

Özet

In this study it was investigated mechanical and wear properties of CAD/CAM restorative materials including feldspathic ceramic, leucite-reinforced glass ceramic, lithium disilicate glass ceramic, and resin-matrix ceramics. The hardness values of materials were measured with micro hardness tester. Wear properties were evaluated with pin on disk tribometer. Wear volume were measured with optical profilometer. Worn surfaces were examined with Scanning Electron Microscopy. The lowest friction coefficient was obtained from Lava Ultimate. It was observed that the highest wear rate was obtained from the LAVA sample was showing the lowest micro-hardness. The lowest wear rate was obtained from e-max sample which was showing the highest micro-hardness. The glass ceramic materials showed better wear resistance than resin-matrix ceramic materials. © 2020, TUBITAK. All rights reserved.

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/ebyu/14014Resmi atıflarda kullanılan kalıcı adres
DOI
https://doi.org/10.31202/ecjse.593747Yayıncı resmi DOI adresi
Tam Kayıt
AlanDeğerDil
dc.contributor.authorGhahramanzadeh Asl, Hojjat
dc.contributor.authorSağsöz, Ömer
dc.contributor.authorKara, Levent
dc.date.accessioned2026-10-18T20:28:48.839606142Z
dc.date.available2026-10-18T20:28:48.839606142Z
dc.date.issued2020
dc.description.abstractIn this study it was investigated mechanical and wear properties of CAD/CAM restorative materials including feldspathic ceramic, leucite-reinforced glass ceramic, lithium disilicate glass ceramic, and resin-matrix ceramics. The hardness values of materials were measured with micro hardness tester. Wear properties were evaluated with pin on disk tribometer. Wear volume were measured with optical profilometer. Worn surfaces were examined with Scanning Electron Microscopy. The lowest friction coefficient was obtained from Lava Ultimate. It was observed that the highest wear rate was obtained from the LAVA sample was showing the lowest micro-hardness. The lowest wear rate was obtained from e-max sample which was showing the highest micro-hardness. The glass ceramic materials showed better wear resistance than resin-matrix ceramic materials. © 2020, TUBITAK. All rights reserved.
dc.identifier.doi10.31202/ecjse.593747
dc.identifier.eissn2148-3736
dc.identifier.endpage66
dc.identifier.issn2148-3736
dc.identifier.issue1
dc.identifier.scopus2-s2.0-85095958475
dc.identifier.startpage57
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/ebyu/14014
dc.identifier.volume7
dc.language.isoen
dc.publisherTUBITAK
dc.relation.ispartofEl-Cezeri Journal of Science and Engineering
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectCAD/CAM restorative materials
dc.subjectMicro Hardness
dc.subjectWear
dc.titleInvestigation of mechanical and wear properties of five (5) different CAD/CAM restorative materials; [Beş (5) farklı CAD / CAM restoratif malzemelerin mekanik ve aşınma özelliklerinin incelenmesi]
dc.typeArticle
dspace.entity.typePublication
rdl.citation.scopus3
rdl.citation.trdizin1
rdl.departmentİSTANBUL GEDİK ÜNİVERSİTESİ
rdl.departmentATATÜRK ÜNİVERSİTESİ
rdl.departmentERZİNCAN BİNALİ YILDIRIM ÜNİVERSİTESİ
rdl.oa.statusgold
rdl.source.indexSCOPUS
rdl.source.indexTRDIZIN